| Brand Name | ACB | Model Number | 1 liter、3.75 liter、5 liter、18-20 liter | Place of Origin | China | 
|---|
Golden Pearl Topcoat Paint / low temperature baking paint with self dry acrylic resin
Topcoat Paint,  A149 Golden Pearl,  A gold prarl with bright gold face and flop,  frequently used in gold and yellow color.
 
 
Quick Detail:
| Product Type | This low temperature baking paint is used as triple-layer top coat. It features accurate colours, high gloss, high hardness and cubic effect. Easy to apply, it is durable and won’t fade easily. | 
|  Purpose | Polished, completely dry, in good condition original paint, old paint surface and intermediate paint surface. | 
| Substrate | The old paint and all kinds of mediun paint,primer is surface have been hardened and abraded | 
| Mixing Ratio | A149 Golden Pearl 100parts  | 
| Notice | 1, read the instructions before construction;  | 
| Shelf Life | 18months if stored in its original sealed cans at 20℃ | 
| Packing | 1liter , 3.75liter or 5 liter can | 
Specifications:
Specific Gravity : 0.95±0.05kg/L(Varies with different colours)
Viscosity : 110~130S (spray-4 cups)/ 25℃
Ingredients: self-dry acrylic resin , pigment, auxiliary agent, solvent, pearl powder
Colour: different colours available upon request of customers.
 
 
Application  Details:
(1) Substrate Treatment
① Wet-sand the middle-coating paint with 800-grit sand paper. When the paint is dry, spray pearl paint.
② If the there’s old paint film unsuitable for the substrate, it is suggested to use two-component middle-coating blocking primer, otherwise such phenomena as peeling off, bubling and floating would appear.
③ As the pearl paint has a high transparency, usually operators should ensure that the paint film of the middle-coating baking paint is unified in colour and has no sanding mark and grain on it, or the marks and grains would emerge through the pearl paint.
(2) Application Content:
① Dilutiing Proportion: A149 Golden Pearl : thinner★=1: 0.8~1  (★Make a proper thinner proportion according to different temperatures)
② Spray Viscosity: 15~19S(spray-4 cups)/25℃
③ Spray Pressure:4-5 Pa ; 
④ Nozzle Diameter: gravity type 1.2~1.5mm
                                Suction type 1.4-1.6mm
⑤ Spray Coats: 2~3 coats
⑥ Spray Thickness: 15~25μm; 
⑦ Waiting Interval: 5~10 minutes; After the final spray, wait 15-20 minutes before spraying a finish varnish. 
(3) Colour Flexibility: For repairs, adjust the colour using Huantong 1K Series colour master.
(4) Tool Cleanings: Clean with the thinner.
 
Precautionss:
①  As pearl paint may produce colour difference on the surface due to different film
thickness and different spraying methods (dry or wet spray), it is suggested to adopt wetter spray application.
② To spray a pearl paint, using our special-designed thinner can get a better effect.
③ The paint film of pearl paint should never exceed 25μm.
④ To spray pure white pearl paint, you must adopt triple-step spraying method. 
⑤ Spray a finish varnish 15-20 minutes after spraying the metallic paint. The longest interval should never exceed 2 hours.